Preparation before operation
1. Check the material: Make sure that the gold foil coil is free of creases and pollution, and the edge of the coil is neat
2. Equipment inspection: confirm the sharpness of the slitting blade and check whether the air pressure system is normal
3. Environmental control: keep the working environment clean, with appropriate temperature and humidity (recommended temperature 20-25°C, humidity 40-60%)

Common problems and solutions
1. Burr/irregular edges
• Possible cause: Blade passivation or improper installation
• Solution:
◦ Replace or sharpen the blade
◦ Adjust blade pressure (0.2-0.3MPa recommended)
◦ Check the tension of the gold foil roll (keep it uniform and moderate)
2. The slitting size is not accurate
• Possible causes: Loose mechanical drivetrain or faulty encoder
• Solution:
◦ Calibrate the slitting size setting
◦ Inspect and tighten transmission components
◦ Clean the encoder or contact a technician for service

3. The material is wrinkled
• Possible causes: uneven tension or unbalanced guide rollers
• Solution:
◦ Adjust the unwinding and rewinding tension
◦ Check the parallelism and levelness of all guide rollers
◦ Reduced slitting speed (especially thin gold leaf)
4. Slitting surface adhesion
• Possible causes: Static build-up or high temperature
• Solution:
◦ Install the static eliminator
◦ Reduce the temperature of the workshop
◦ Appropriate reduction of winding pressure

Routine maintenance recommendations
1. Clean the blades and guide rollers every 8 hours
2. Inspect the air system and transmission components weekly
3. Fully calibrate the accuracy of the equipment every month
4. Change the lubricating oil and filters quarterly
Safety Precautions
• Wear protective gloves and goggles when operating
• It is forbidden to touch moving parts with your hands while the equipment is running
• Press the E-STOP button immediately in case of emergency
• Inspect electrical safety devices regularly
Following these guidelines can significantly reduce slitting problems and improve production efficiency and product quality.
Hot Stamping Foil Slitting Machine Maintenance Guide: Solving issues such as burrs, misalignment, and foil breakage03. September, 2026
Maintenance interval for the hot stamping foil slitting machine: daily/weekly/monthly/yearly standard02. September, 2026